Customization: | Available |
---|---|
Color: | White |
Material: | Ceramics |
Still deciding? Get samples of US$ 5/Piece
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
|
---|---|
Support payments in USD |
Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Porous ceramic balls is also called filtering balls. It is made by make 20-30% pores inside the inert ceramic balls. Therefore it can be used not only for supporting and covering the catalyst, but also for filtering and eliminating the impurities of grain, gelatin, asphalting, heavy metal and iron ions of less than 25um. If the porous ball is set on the top of a reactor, the impurities fail to be eliminated in former process could be adsorbed in the pores inside the balls, there upon protect the catalyst and prolong the operating cycle of the system.As the impurities present in the materials are different, the user can select the product by their sizes, pores and porosity, or if necessary, add molybdenum, nickel and cobalt or other active components to prevent the catalyst from coking or poisoning.
Type | Feldspar | Feldspar- Molai | Molai Stone | Molai- Corundum | Corundum | |||||
Item | ||||||||||
Chemical Content (%) |
Al2O3 | 20-30 | 30-45 | 45-70 | 70-90 | ≥90 | ||||
Al2O3+ SiO2 | ≥90 | |||||||||
Fe2O3 | ≤1 | |||||||||
Water Adsorption (%) | ≤5 | |||||||||
Acid Resistance (%) | ≥98 | |||||||||
Alkaki Resistance (%) | ≥80 | ≥82 | ≥85 | ≥90 | ≥95 | |||||
Operation Temperature(°C) | ≥1300 | ≥1400 | ≥1500 | ≥1600 | ≥1700 | |||||
Crushing Strength (N/Piece) |
Φ3mm | ≥400 | ≥420 | ≥440 | ≥480 | ≥500 | ||||
Φ6mm | ≥480 | ≥520 | ≥600 | ≥620 | ≥650 | |||||
Φ8mm | ≥600 | ≥700 | ≥800 | ≥900 | ≥1000 | |||||
Φ10mm | ≥1000 | ≥1100 | ≥1300 | ≥1500 | ≥1800 | |||||
Φ13mm | ≥1500 | ≥1600 | ≥1800 | ≥2300 | ≥2600 | |||||
Φ16mm | ≥1800 | ≥2000 | ≥2300 | ≥2800 | ≥3200 | |||||
Φ20mm | ≥2500 | ≥2800 | ≥3200 | ≥3600 | ≥4000 | |||||
Φ25mm | ≥3000 | ≥3200 | ≥3500 | ≥4000 | ≥4500 | |||||
Φ30mm | ≥4000 | ≥4500 | ≥5000 | ≥5500 | ≥6000 | |||||
Φ38mm | ≥6000 | ≥6500 | ≥7000 | ≥8500 | ≥10000 | |||||
Φ50mm | ≥8000 | ≥8500 | ≥9000 | ≥10000 | ≥12000 | |||||
Φ75mm | ≥10000 | ≥11000 | ≥12000 | ≥14000 | ≥15000 | |||||
Bulk Density (kg/m3) | 1100-1200 | 1200-1300 | 1300-1400 | 1400-1550 | ≥1550 |
Type | Feldspar | Feldspar- Molai | Molai Stone | Molai- Corundum | Corundum | |||||
Item | ||||||||||
Chemical Content (%) |
Al2O3 | 20-30 | 30-45 | 45-70 | 70-90 | ≥90 | ||||
Al2O3+ SiO2 | ≥90 | |||||||||
Fe2O3 | ≤1 | |||||||||
Water Adsorption (%) | ≤5 | |||||||||
Acid Resistance (%) | ≥98 | |||||||||
Alkaki Resistance (%) | ≥80 | ≥82 | ≥85 | ≥90 | ≥95 | |||||
Operation Temperature(°C) | ≥1300 | ≥1400 | ≥1500 | ≥1600 | ≥1700 | |||||
Crushing Strength (N/Piece) |
Φ3mm | ≥400 | ≥420 | ≥440 | ≥480 | ≥500 | ||||
Φ6mm | ≥480 | ≥520 | ≥600 | ≥620 | ≥650 | |||||
Φ8mm | ≥600 | ≥700 | ≥800 | ≥900 | ≥1000 | |||||
Φ10mm | ≥1000 | ≥1100 | ≥1300 | ≥1500 | ≥1800 | |||||
Φ13mm | ≥1500 | ≥1600 | ≥1800 | ≥2300 | ≥2600 | |||||
Φ16mm | ≥1800 | ≥2000 | ≥2300 | ≥2800 | ≥3200 | |||||
Φ20mm | ≥2500 | ≥2800 | ≥3200 | ≥3600 | ≥4000 | |||||
Φ25mm | ≥3000 | ≥3200 | ≥3500 | ≥4000 | ≥4500 | |||||
Φ30mm | ≥4000 | ≥4500 | ≥5000 | ≥5500 | ≥6000 | |||||
Φ38mm | ≥6000 | ≥6500 | ≥7000 | ≥8500 | ≥10000 | |||||
Φ50mm | ≥8000 | ≥8500 | ≥9000 | ≥10000 | ≥12000 | |||||
Φ75mm | ≥10000 | ≥11000 | ≥12000 | ≥14000 | ≥15000 | |||||
Bulk Density (kg/m3) | 1100-1200 | 1200-1300 | 1300-1400 | 1400-1550 | ≥1550 |